IRON TUNGSTEN COATING FORMULATIONS AND PROCESSES

Last updated:

Abstract:

An electrolyte solution for iron-tungsten plating is prepared by dissolving in an aqueous medium a divalent iron salt (e.g., iron (II) sulfate) and an alkali metal citrate (e.g., sodium citrate, potassium citrate, or other alkali metal citrate) to form a first solution, dissolving in the first solution a tungstate salt (e.g., sodium tungstate, potassium tungstate, or other potassium tungstate) to form a second solution, and dissolving in the second solution a citric acid to form the electrolyte solution. An iron-tungsten coating is formed on a substrate using the electrolyte solution by passing a current between a cathode and an anode through the electrolyte solution to deposit iron and tungsten on the substrate.