SEAL COATS TO PREVENT SILICON LOSS DURING RE-MELT INFILTRATION OF SI CONTAINING COMPOSITES
Last updated:
Abstract:
Provided is a method including obtaining ceramic matrix composite (CMC) with a first matrix portion including a silicon carbide and silicon phase dispersed therewithin, disposing a coating thereupon to form a sealed part, and forming thereupon another segment comprising a CMC, which may be another matrix portion including a silicon carbide and a silicon phase dispersed within therewithin. Also provided is a gas turbine component with a CMC segment including a matrix portion including a silicon carbide and a silicon phase dispersed therewithin, a sealing layer including silicon carbide enclosing the first segment, and a second segment on the sealing layer, wherein the second segment includes a melt-infiltrated CMC having a matrix portion including a silicon carbide and a silicon phase dispersed therewithin.