Abstract:
A method of forming an optical fiber, including: exposing a soot core preform to a dopant gas at a pressure of from 1.5 atm to 40 atm, the soot core preform comprising silica, the dopant gas comprising a first halogen doping precursor and a second halogen doping precursor, the first halogen doping precursor doping the soot core preform with a first halogen dopant and the second halogen precursor doping the soot core preform with a second halogen dopant; and sintering the soot core preform to form a halogen-doped closed-pore body, the halogen-doped closed-pore body having a combined concentration of the first halogen dopant and the second halogen dopant of at least 2.0 wt %.
Status:
Grant
Type:
Utility
Filling date:
1 Aug 2019
Issue date:
16 Nov 2021