A single mode optical fiber is provided that includes a core region and a cladding region, the cladding region including a depressed-index cladding region, a first outer cladding region, and a second outer cladding region. The first outer cladding region has a lower relative refractive than the second outer cladding region. The single mode optical fiber has a bend loss at 1550 nm for a 15 mm diameter mandrel of less than about 0.75 dB/turn, has a bend loss at 1550 nm for a 20 mm diameter mandrel of less than about 0.2 dB/turn, and a bend loss at 1550 nm for a 30 mm diameter mandrel of less than about 0.005 dB/turn. Additionally, the single mode optical fiber has a mode field diameter of about 9.0 microns or greater at 1310 nm wavelength and a cable cutoff of less than or equal to about 1260 nm.