Corning Incorporated
CHEMICALLY STRENGTHENABLE MACHINABLE GLASS-CERAMICS

Last updated:

Abstract:

A glass-ceramic comprising, in weight percent on an oxide basis, of 50 to 70% SiO.sub.2, 0 to 20% Al.sub.2O.sub.3, 12 to 23% MgO, 0 to 4% Li.sub.2O, 0 to 10% Na.sub.2O, 0 to 10% K.sub.2O, 0 to 5% ZrO.sub.2, and 2 to 12% F, wherein the predominant crystalline phase of said glass-ceramic is a trisilicic mica, a tetrasilicic mica, or a mica solid solution between trisilicic and tetrasilicic, and wherein the total of Na.sub.2O+Li.sub.2O is at least 2 wt. %; wherein the glass-ceramic can be ion-exchanged.

Status:
Application
Type:

Utility

Filling date:

18 Mar 2020

Issue date:

20 Jan 2022