Corning Incorporated
Fictivated glass and method of making
Last updated:
Abstract:
Silicate glasses that are fictivated and fast cooled and have high levels of intrinsic or "native" damage resistance. When ion exchanged, the silicate glasses described herein have a Vickers crack initiation threshold of at least 15 kgf and, in some embodiments, at least about 25 kgf.
Status:
Grant
Type:
Utility
Filling date:
28 Jan 2014
Issue date:
3 Dec 2019