Eastman Kodak Company
Method of making silver-containing dispersions

Last updated:

Abstract:

A method is used to prepare silver nanoparticles or copper nanoparticles in the form of a silver nanoparticle cellulosic polymeric composite or a copper nanoparticle cellulose polymeric composite, respectively. A cellulosic polymer, organic solvent having a boiling point at atmospheric pressure of 100.degree. C. to 500.degree. C. and a Hansen parameter (.delta..sub.T.sup.Polymer) equal to or greater than that of the cellulosic polymer, ascorbic acid, and a nitrogenous base are mixed to form a premix solution. At room temperature or upon heating the premix solution to a temperature of at least 40.degree. C., a solution of reducible silver ions or reducible copper ions is added. The resulting silver or copper nanoparticle composite is cooled, isolated, and re-dispersed in an organic solvent, providing a non-aqueous silver-containing or copper-containing dispersion that can be disposed on a substrate to form an article.

Status:
Grant
Type:

Utility

Filling date:

8 Nov 2017

Issue date:

12 Nov 2019