Eastman Kodak Company
Yarn with coating over yarn core

Last updated:

Abstract:

A coated yarn has a yarn core and a coating disposed coaxially on the yarn core. This coating contains: (i) porous particles present in an amount of at least 4 weight % and up to and including 20 weight %, each porous particle comprising a continuous polymeric phase and discrete pores dispersed within the continuous polymeric phase, having a mode particle size of 2-50 .mu.m and up to and including 50 .mu.m; (ii) a film-forming binder material having a T.sub.g of less than or equal to 25.degree. C., which is present in an amount of 40-90 weight %; and (iii) an inorganic filler material having a value of less than 5 on the MOHS scale of mineral hardness, which inorganic filler material is present in an amount of 4 weight % and up to and including 30 weight %.

Status:
Grant
Type:

Utility

Filling date:

29 Nov 2018

Issue date:

17 Aug 2021