PROCESS FOR LOW-COST TEMPERING OF ALUMINUM CASTING
Last updated:
Abstract:
A thermally stable component formed of a tempered aluminum alloy casting which reduced costs is provided. The aluminum alloy typically has an elongation of at least 8% after casting, which is preferred for self-piercing rivet processes. The aluminum alloy leaves a casting facility in the as-cast (F temper) condition. The cast aluminum alloy is then shipped to another entity, such as an OEM, and is subjected to an artificial aging process, such as on the OEM's existing paint line, rather than at the casting facility. The artificial aging process typically includes electrodeposition coating and curing. The components that can be formed by the reduced cost method include lightweight automotive vehicle components, including structural, body-in-white, suspension, or chassis components, such as front shock towers, front body hinge pillars, tunnels, and rear rails.