POSCO Holdings Inc.
METHOD FOR PRODUCING GRAIN-ORIENTED ELECTRICAL STEEL SHEET
Last updated:
Abstract:
A method for producing a grain-oriented electrical steel sheet according to an embodiment of the present invention comprises the steps of: heating a slab satisfying the following formula 1 and including, by wt %, 3.2 to 4.0% of Si, 0.03 to 0.09% of C, 0.015 to 0.040% of A1, 0.04 to 0.15% of Mn, 0.001 to 0.005% of N, 0.01% or less of S (exclusive of 0%), and the balance of Fe and other inevitable impurities; hot rolling the slab to produce a hot rolled sheet; hot band annealing the hot rolled sheet to at a cracking temperature of 900 to 980.quadrature. for 30 to 300 seconds; cold rolling the hot rolled sheet, which has completely been hot band annealed, to produce a cold rolled sheet; subjecting the cold rolled sheet to primary recrystallization annealing; and conducting secondary recrystallization annealing for the cold rolled sheet which has completely been primary recrystallization annealed. [Mn].times.[S].ltoreq.0.0004 [Formula 1] (wherein [Mn] and [S] are contents (wt %) of Mn and S in the slab, respectively.)
Utility
21 Dec 2017
30 Jan 2020