POLYETHYLENE RECYCLABLE FILM WITH HIGH STRENGTH AND/OR BARRIER

Last updated:

Abstract:

Polyethylene recyclable composite article comprises multilayer film having first layer comprising polyolefin with a melting point .ltoreq.190.degree. C., second layer comprising second polymer selected from amorphous polyamide, polyamide with melt point 191-205.degree. C., polyvinylidene chloride w/melt point 191-205.degree. C., and/or EVOH w/melt point 191-205.degree. C., and tie layer between the first layer and the second layer. The multilayer film is bonded to itself or another component. The second polymer makes up 1 to 10 wt % of composite article weight, and composite article exhibits a composite melt index of from 0.5 to 4 grams/10 min at 190.degree. C. and 2.16 kg in a Composite Melt Index Test. A corresponding polyethylene recyclable multilayer film also exhibits 0.5 to 4 grams/10 min at 190.degree. C. and 2.16 kg in a Composite Melt Index Test.

Status:
Application
Type:

Utility

Filling date:

6 Mar 2019

Issue date:

31 Dec 2020