Texas Instruments Incorporated
METHOD OF REDUCING VOIDS AND SEAMS IN TRENCH STRUCTURES BY FORMING SEMI-AMORPHOUS POLYSILICON

Last updated:

Abstract:

A microelectronic device with a trench structure is formed by forming a trench in a substrate, forming a seed layer in the trench, the seed layer including an amorphous dielectric material; and forming semi-amorphous polysilicon on the amorphous dielectric material. The semi-amorphous polysilicon has amorphous silicon regions separated by polycrystalline silicon. Subsequent thermal processes used in fabrication of the microelectronic device may convert the semi-amorphous polysilicon in the trench to a polysilicon core. In one aspect, the seed layer may be formed on sidewalls of the trench, contacting the substrate. In another aspect, a polysilicon outer layer may be formed in the trench before forming the seed layer, and the seed layer may be formed on the polysilicon layer.